MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Celcon® MT24F01 Medical Grade Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes: Description: Celcon acetal copolymer grade MT24F01 is a special grade developed for medical industry applications containing low residual monomers. Celcon MT24F01 is a low level PTFE filled product designed for use in wear applications against plastics, metal, glass or ceramic mating surfaces where silicone lubricants can not be tolerated.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 59.0 MPa8560 psi50 mm/min; ISO 527-2/1A
Flexural Modulus 2.47 GPa358 ksiISO 178
Izod Impact, Notched (ISO) 4.30 kJ/m²2.05 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C210 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 199 °C360 - 390 °F
Mold Temperature 77.0 - 93.0 °C171 - 199 °F
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Injection Pressure 75.8 - 110 MPa11000 - 16000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® MT8U01 Medical Grade Acetal Copolymer
Celanese Celcon® MT12U03 Medical Grade Acetal Copolymer
Celanese Celcon® MT24U01 Medical Grade Acetal Copolymer
LG Chemical MP211 ABS, Low Gloss, Metal Plating
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic

PHCW31 / 45972

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.