MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Universal Wire Works E81T1-Ni1 Flux Cored Carbon Steel Tubular Electrode
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multiple pass welding have a spray-like transfer with very little spatter. The fast freezing slag facilitates welding in all positions and is easily removed. Alloy 81T1-Ni1 is formulated for welding ASTM A572, A302, A588, and A734. These steels are used in the fabrication of transmission poles, light poles, earth moving and mining machinery and offshore platforms. Alloy 81T1-Ni2 is formulated for welding ASTM A572, A575, and A734. The combination of strength and CVN toughness of Ni-2 make it ideal for applications such as offshore platform construction, shipbuilding, earthmoving and mining equipment.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS A5.29 E81T1-Ni1; ASME SFA-5.29 E81T1-Ni1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 576 MPa83500 psi
Tensile Strength, Yield 530 MPa76900 psi
Elongation at Break 24 %24 %
Charpy Impact 40.7 J
@Temperature -28.9 °C
30.0 ft-lb
@Temperature -20.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.030 %0.030 %
Iron, Fe 97.6 %97.6 %As remainder
Manganese, Mn 0.80 %0.80 %
Nickel, Ni 1.0 %1.0 %
Phosphorus, P 0.12 %0.12 %
Silicon, Si 0.35 %0.35 %
Sulfur, S 0.15 %0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NUWW170 / 19671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.