MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
347 Stainless Steel, annealed
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Niobium plus Tantalum is ten times the minimum carbon content

Key Words: AFNOR Z 6 CNNb 18.10, UNI X 8 CrNiNb 18 11, JIS SUS 347, SS14 2338 (Sweden), UNS S34700, AMS 5512, AMS 5556, AMS 5558, AMS 5571, AMS 5575, AMS 5646, AMS 5654, AMS 5674, AMS 5680, AMS 5681, ASME SA182, ASME SA193, ASME SA194, austenitic, ASME SA213, ASME SA240, ASME SA249, ASME SA312, ASME SA320 (B8C), ASME SA358, ASME SA376, ASME SA403, ASME SA409, ASME SA430, ASME SA473, ASME SA479, ASME SA493, ASME SA511, ASME SA554, ASME SA580, ASME SA633, FED QQ-S-763, FED QQ-S-766, B.S. 347 S 17, B.S. En. 58 F, B.S. En. 58 G, B.S. ANC 3 Grade B, FED QQ-W-423, MIL SPEC MIL-S-862, MIL SPEC MIL-S-23196, SAE J405 (30347), DIN 1.4550, ISO 683/13 16
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 620 MPa
 69.0 MPa
@Temperature 1040 °C
 83.0 MPa
@Temperature 980 °C
 105 MPa
@Temperature 925 °C
 140 MPa
@Temperature 870 °C
 170 MPa
@Temperature 815 °C
 215 MPa
@Temperature 760 °C
 275 MPa
@Temperature 705 °C
 330 MPa
@Temperature 650 °C
 380 MPa
@Temperature 595 °C
 405 MPa
@Temperature 540 °C
 435 MPa
@Temperature 480 °C
 455 MPa
@Temperature 425 °C
 470 MPa
@Temperature 370 °C
 495 MPa
@Temperature 315 °C
 510 MPa
@Temperature 260 °C
 525 MPa
@Temperature 205 °C
 540 MPa
@Temperature 150 °C
 580 MPa
@Temperature 95.0 °C
Tensile Strength, Yield 255 MPa
@Strain 0.2 %
 83.0 MPa
@Strain 0.2 %,
Temperature 925 °C
 105 MPa
@Strain 0.2 %,
Temperature 870 °C
 115 MPa
@Strain 0.2 %,
Temperature 815 °C
 130 MPa
@Strain 0.2 %,
Temperature 760 °C
 140 MPa
@Strain 0.2 %,
Temperature 595 °C
 140 MPa
@Strain 0.2 %,
Temperature 650 °C
 140 MPa
@Strain 0.2 %,
Temperature 705 °C
 145 MPa
@Strain 0.2 %,
Temperature 480 °C
 145 MPa
@Strain 0.2 %,
Temperature 540 °C
 150 MPa
@Strain 0.2 %,
Temperature 425 °C
 160 MPa
@Strain 0.2 %,
Temperature 370 °C
 170 MPa
@Strain 0.2 %,
Temperature 315 °C
 195 MPa
@Strain 0.2 %,
Temperature 260 °C
 205 MPa
@Strain 0.2 %,
Temperature 205 °C
 240 MPa
@Strain 0.2 %,
Temperature 150 °C
 250 MPa
@Strain 0.2 %,
Temperature 95.0 °C
Elongation at Break 50 %in 50 mm
 34 %
@Temperature 480 °C
in 50 mm
 34 %
@Temperature 540 °C
in 50 mm
 35 %
@Temperature 595 °C
in 50 mm
 35 %
@Temperature 315 °C
in 50 mm
 35 %
@Temperature 370 °C
in 50 mm
 35 %
@Temperature 425 °C
in 50 mm
 36 %
@Temperature 650 °C
in 50 mm
 36 %
@Temperature 705 °C
in 50 mm
 36 %
@Temperature 260 °C
in 50 mm
 37 %
@Temperature 760 °C
in 50 mm
 38 %
@Temperature 205 °C
in 50 mm
 40 %
@Temperature 815 °C
in 50 mm
 40 %
@Temperature 870 °C
in 50 mm
 42 %
@Temperature 150 °C
in 50 mm
 45 %
@Temperature 95.0 °C
in 50 mm
 45 %
@Temperature 925 °C
in 50 mm
 50 %
@Temperature 980 °C
in 50 mm
 60 %
@Temperature 1040 °C
in 50 mm
Modulus of Elasticity 195 GPa
Poissons Ratio 0.27
Shear Modulus 77.0 GPa
Izod Impact 120 - 160 J
Charpy Impact 160 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.008at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 260 °C
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1425 °C
Solidus 1400 °C
Liquidus 1425 °C
Maximum Service Temperature, Air 870 °CIntermittent
 925 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 17 %
Iron, Fe 68 %
Manganese, Mn <= 2.0 %
Nb + Ta 0.80 %
Nickel, Ni 11 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
347 Stainless Steel, annealed, bar
304 Stainless Steel
347 Stainless Steel, annealed and cold drawn, bar
347 Stainless Steel, annealed, plate
321H Austenitic Stainless Steel (UNS S32109)

MQ347AT / 12856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.