DuPont™ Elvax® 4320 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications. ApplicationsElvax® 4320 resins can be used for the following applications: adhesives, sealants, and wax blends. Information provided by DuPont™ This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition. |