MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 2515 Steel (UNS G25150)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Key Words: UNS G25150
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 233233
Tensile Strength, Ultimate 779 MPa113000 psi
Tensile Strength, Yield 648 MPa
@Strain 0.2 %
94000 psi
@Strain 0.2 %
Elongation at Break 25 %25 %
Modulus of Elasticity 201 - 209 GPa29200 - 30300 ksi
Bulk Modulus 160 - 170 GPa23200 - 24700 ksi
Poissons Ratio 0.27 - 0.300.27 - 0.30
Shear Modulus 81.0 - 82.0 GPa11700 - 11900 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear >= 10.9 µm/m-°C>= 6.06 µin/in-°F
Thermal Conductivity 34.3 W/m-K238 BTU-in/hr-ft²-°F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 2330 Steel (UNS G23300)
AISI 3140
AISI 3120 Steel (UNS G31200)
AISI 3150 Steel (UNS G31500)
AISI 1330 Steel

M2515 / 100229

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.