MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Bada BADAMID® A702 GF25 FR HF uncolored Nylon 66, 25% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: flame retardant (red phosphorus), 25% glass fibers reinforced and heat stabilized injection molding grade with excellent electrical properties

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183
Moisture Absorption 1.30 %1.30 %50% r.h.; ISO 62
Water Absorption at Saturation 5.7 %5.7 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 190 MPa
@Load 36.5 kg
27600 psi
@Load 80.5 lb
ISO 2039-1
Tensile Strength at Break 140 MPa20300 psi5 mm/min; ISO 527-1/2
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527-1/2
Tensile Modulus 9.20 GPa1330 ksi1 mm/min; ISO 527-1/2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC-62631-3-1
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC-62631-3-2
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC-62631-2-1
Dielectric Strength 33.0 kV/mm838 kV/inIEC-60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC-62631-2-1
Comparative Tracking Index 600 V600 VIEC-60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °F10 K/min; ISO 3146
Maximum Service Temperature, Air 220 °C428 °Fsome hours; EC-60216
 130 °C
@Time 7.20e+7 sec
266 °F
@Time 20000 hour
EC-60216
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-1/2
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Glow Wire Ignition Temperature 800 °C
@Thickness 1.00 mm
1470 °F
@Thickness 0.0394 in
IEC-60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC-60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBADA060 / 286893

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.