MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) REPEL-O-TEX® SRP-6 Surfactant
Categories: Fluid

Material Notes: Standard Applications: REPEL-O-TEX SRP-6 is a polymer offering protection against the adhesion of greasy soils to polyester fabrics after two wash cycles.

Chemical Name: Polyethylene Glycol Polyester

CAS No: 9016-88-0

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.600 g/cc0.0217 lb/in³
Water Absorption <= 3.0 %<= 3.0 %1 hr @ 105°C; RP-0540
Particle Size <= 300 µm<= 300 µm20%
 300 - 850 µm300 - 850 µm60%
 850 - 1180 µm850 - 1180 µm20%
 >= 1180 µm>= 1180 µm<1%
pH 4.0 - 8.04.0 - 8.01% dispersion in water; RP-0420
Viscosity <= 3000 cP
@Temperature 176 °C
<= 3000 cP
@Temperature 349 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceClear GranulesRP-0064
Content>97%Polymer
Saponification number98-109[mg KOH/g], RP-0496

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLVAY762 / 218490

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.