MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay Chemicals Perchloroethylene
Categories: Fluid; Solvent

Material Notes: Perchloroethylene is a non-flammable product

EINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.617 - 1.621 g/cc0.05842 - 0.05856 lb/in³D25/25
 1.474 g/cc
@Temperature 110 °C
0.05325 lb/in³
@Temperature 230 °F
 1.475 g/cc
@Temperature 120 °C
0.05329 lb/in³
@Temperature 248 °F
 1.49 g/cc
@Temperature 100 °C
0.0538 lb/in³
@Temperature 212 °F
 1.507 g/cc
@Temperature 90.0 °C
0.05444 lb/in³
@Temperature 194 °F
 1.523 g/cc
@Temperature 80.0 °C
0.05502 lb/in³
@Temperature 176 °F
 1.54 g/cc
@Temperature 70.0 °C
0.0556 lb/in³
@Temperature 158 °F
 1.557 g/cc
@Temperature 60.0 °C
0.05625 lb/in³
@Temperature 140 °F
 1.573 g/cc
@Temperature 50.0 °C
0.05683 lb/in³
@Temperature 122 °F
 1.59 g/cc
@Temperature 40.0 °C
0.0574 lb/in³
@Temperature 104 °F
 1.598 g/cc
@Temperature 35.0 °C
0.05773 lb/in³
@Temperature 95.0 °F
 1.606 g/cc
@Temperature 30.0 °C
0.05802 lb/in³
@Temperature 86.0 °F
 1.615 g/cc
@Temperature 25.0 °C
0.05835 lb/in³
@Temperature 77.0 °F
 1.623 g/cc
@Temperature 20.0 °C
0.05863 lb/in³
@Temperature 68.0 °F
 1.631 g/cc
@Temperature 15.0 °C
0.05892 lb/in³
@Temperature 59.0 °F
 1.64 g/cc
@Temperature 10.0 °C
0.0592 lb/in³
@Temperature 50.0 °F
 1.646 g/cc
@Temperature 0.000 °C
0.05947 lb/in³
@Temperature 32.0 °F
 1.648 g/cc
@Temperature 5.00 °C
0.05954 lb/in³
@Temperature 41.0 °F
Viscosity  0.41 cP
@Temperature 110 °C
0.41 cP
@Temperature 230 °F
Dynamic
 0.44 cP
@Temperature 100 °C
0.44 cP
@Temperature 212 °F
Dynamic
 0.48 cP
@Temperature 90.0 °C
0.48 cP
@Temperature 194 °F
Dynamic
 0.51 cP
@Temperature 80.0 °C
0.51 cP
@Temperature 176 °F
Dynamic
 0.56 cP
@Temperature 70.0 °C
0.56 cP
@Temperature 158 °F
Dynamic
 0.61 cP
@Temperature 60.0 °C
0.61 cP
@Temperature 140 °F
Dynamic
 0.66 cP
@Temperature 50.0 °C
0.66 cP
@Temperature 122 °F
Dynamic
 0.68 cP
@Temperature 120 °C
0.68 cP
@Temperature 248 °F
Dynamic
 0.73 cP
@Temperature 40.0 °C
0.73 cP
@Temperature 104 °F
Dynamic
 0.76 cP
@Temperature 35.0 °C
0.76 cP
@Temperature 95.0 °F
Dynamic
 0.80 cP
@Temperature 30.0 °C
0.80 cP
@Temperature 86.0 °F
Dynamic
 0.84 cP
@Temperature 25.0 °C
0.84 cP
@Temperature 77.0 °F
Dynamic
 0.89 cP
@Temperature 20.0 °C
0.89 cP
@Temperature 68.0 °F
Dynamic
 0.94 cP
@Temperature 15.0 °C
0.94 cP
@Temperature 59.0 °F
Dynamic
 0.99 cP
@Temperature 10.0 °C
0.99 cP
@Temperature 50.0 °F
Dynamic
 1.05 cP
@Temperature 5.00 °C
1.05 cP
@Temperature 41.0 °F
Dynamic
 1.11 cP
@Temperature 0.000 °C
1.11 cP
@Temperature 32.0 °F
Dynamic
Molecular Weight 165.8 g/mol165.8 g/mol
Vapor Pressure  0.00600 bar
@Temperature 0.000 °C
4.50 torr
@Temperature 32.0 °F
 0.00800 bar
@Temperature 5.00 °C
6.00 torr
@Temperature 41.0 °F
 0.0110 bar
@Temperature 10.0 °C
8.25 torr
@Temperature 50.0 °F
 0.0140 bar
@Temperature 15.0 °C
10.5 torr
@Temperature 59.0 °F
 0.0190 bar
@Temperature 20.0 °C
14.3 torr
@Temperature 68.0 °F
 0.0250 bar
@Temperature 25.0 °C
18.8 torr
@Temperature 77.0 °F
 0.0320 bar
@Temperature 30.0 °C
24.0 torr
@Temperature 86.0 °F
 0.0410 bar
@Temperature 35.0 °C
30.8 torr
@Temperature 95.0 °F
 0.0530 bar
@Temperature 40.0 °C
39.8 torr
@Temperature 104 °F
 0.0830 bar
@Temperature 50.0 °C
62.3 torr
@Temperature 122 °F
 0.128 bar
@Temperature 60.0 °C
96.0 torr
@Temperature 140 °F
 0.190 bar
@Temperature 70.0 °C
143 torr
@Temperature 158 °F
 0.275 bar
@Temperature 80.0 °C
206 torr
@Temperature 176 °F
 0.389 bar
@Temperature 90.0 °C
292 torr
@Temperature 194 °F
 0.540 bar
@Temperature 100 °C
405 torr
@Temperature 212 °F
 0.733 bar
@Temperature 110 °C
550 torr
@Temperature 230 °F
 0.979 bar
@Temperature 120 °C
734 torr
@Temperature 248 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  0.840 J/g-°C
@Temperature 0.000 °C
0.201 BTU/lb-°F
@Temperature 32.0 °F
 0.850 J/g-°C
@Temperature 20.0 °C
0.203 BTU/lb-°F
@Temperature 68.0 °F
 0.870 J/g-°C
@Temperature 40.0 °C
0.208 BTU/lb-°F
@Temperature 104 °F
 0.880 J/g-°C
@Temperature 60.0 °C
0.210 BTU/lb-°F
@Temperature 140 °F
 0.900 J/g-°C
@Temperature 80.0 °C
0.215 BTU/lb-°F
@Temperature 176 °F
 0.910 J/g-°C
@Temperature 100 °C
0.217 BTU/lb-°F
@Temperature 212 °F
 0.930 J/g-°C
@Temperature 120 °C
0.222 BTU/lb-°F
@Temperature 248 °F
Distillation Temperature 110.6 - 121.6 °C231.1 - 250.9 °F
 
Descriptive Properties
AppearanceClear without suspended matterASMT D3741/B
Color<10APHA
Composition<1 mg/kgChlorides (Cl)
 <10 mg/kgAdditive (Stabilizer)
 <10 mg/kgNon volatile Residue
 <15 mg/kgOrganically combined Oxygen and Nitrogen
 <25 mg/kgMoisture (H2O), Karl Fischer, ASTM E1064
Purity>999.5 g/kgwithout stabilizers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Chemicals Glycerol alpha monochlorohydrin
Solvay Chemicals SOLVOKANE®
Solvay Chemicals NOCOLOK® Binder (water-based)

WSOLV144 / 147793

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.