MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow ENGAGE™ 8452 EL Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: ENGAGE™ 8452 EL Polyolefin Elastomer is an ethylene-octene copolymer that offers excellent toughness and softness. It has excellent compatibility with other polyolefins, allowing for efficient blending and coextrusion. It provides excellent flow properties and is efficiently cross-linked by peroxide, silane, or irradiation. When cross-linked, it gives exceptional heat aging, compression set, and weather resistance properties.
Main Characteristics:
  • Pellet form
  • Good clarity, toughness, and flexibility
  • Excellent compatibility with other olefins
  • Exceptional heat aging, compression set, and weather resistance when cured
Applications:
  • Wire and cable
Availability: Asia Pacific; Europe; North America

Uses: Blending; Compounding; Low Voltage Insulation; Medium Voltage Insulation; Wire & Cable Applications

Agency Ratings: FDA 21 CFR 177.1520 ©3.2c; EU No 10/2011; JHOSPA

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.877 g/ccASTM D792
Mooney Viscosity 11
@Temperature 121 °C
ML1+4; ASTM D1646
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
@Time 1.00 sec
Compression Molded; ASTM D2240
Hardness, Shore D 24
@Time 1.00 sec
Compression Molded; ASTM D2240
Tensile Strength at Break 1620 psiCompression Molded, 20 in/min; ASTM D638
Elongation at Break 950 %Compression Molded, 20 in/min; ASTM D638
Tensile Modulus 435 psi100% Secant, 20 in/min, Compression Molded; ASTM D638
Flexural Modulus 2390 psi2% Secant, Compression Molded; ASTM D790
 2440 psi1% Secant, Compression Molded; ASTM D790
Tear Strength 258 pliDie C; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Melting Point 151 °F
Crystallization Temperature 118 °FPeak
Vicat Softening Point 118 °FASTM D1525
Glass Transition Temp, Tg -59.8 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF523 / 311216

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.