MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional Stability

Application: E&E (Switch)

CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0090 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.9 MPa
@Thickness 3.20 mm
8110 psi
@Thickness 0.126 in
5mm/min; ASTM D638
Elongation at Break 3.0 %
@Thickness 3.20 mm
3.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Yield Strength 83.4 MPa
@Thickness 3.20 mm
12100 psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus 2.94 GPa
@Thickness 3.20 mm
427 ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched 0.588 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.10 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
660 kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 175 V175 VSolution A; IEC 60112
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
 30 - 60 sec
@Thickness >=3.00 mm
30 - 60 sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI  30 - 60 arcs
@Thickness 3.00 mm
30 - 60 arcs
@Thickness 0.118 in
 60 - 120 arcs
@Thickness 1.50 mm
60 - 120 arcs
@Thickness 0.0591 in
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/min
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FPeak at Break
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
@Thickness 6.40 mm
230 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
Flammability, UL94  V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 225 - 235 °C437 - 455 °FInjection Molding
Middle Barrel Temperature 230 - 245 °C446 - 473 °FInjection Molding
Front Barrel Temperature 240 - 250 °C464 - 482 °FInjection Molding
Nozzle Temperature 240 - 250 °C464 - 482 °FInjection Molding
Melt Temperature 240 - 250 °C464 - 482 °FInjection Molding
Mold Temperature 60.0 - 90.0 °C140 - 194 °FInjection Molding
Drying Temperature 100 °C212 °FInjection Molding
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mid-Mountain Materials ARMATEX® SF7 Silicone Rubber Coated Glass Fabric

PLAY451 / 148461

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.