MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Carpenter R.D.S.® Alloy Tool Steel (Oil-Hard) (AISI L6)
Categories: Metal; Ferrous Metal; Tool Steel; Oil-Hardening Steel

Material Notes: R.D.S. tool steel is an oil hardening die steel which combines extreme toughness with very little size change when heat treated. It is available as a DeCarb-Free product. DCF bars have been cold finished in the mill, eliminating the need for bar bark removal.

Applications: Hobs, Collets, Punches, Forming Rolls, Blanking or forming dies, Thread roller dies, Embossing dies, Shear blades, Stamps, Swaging dies, Slitting shears, Slitting cutters, Clutch parts, Pawls, Dogs, Stops, Knuckle Pins, Spindles, Fingers, Indexing pins, Clutch pins

Information provided by Carpenter Technology Corporation.

R.D.S.® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS T61206
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.86 g/cc7.86 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 45 - 4645 - 46Tempered at 800°F
 61 - 6261 - 62As hardened
Tensile Strength, Ultimate 1950 MPa283000 psiwhen tempered at 400°F
Tensile Strength, Yield 1910 MPa277000 psiwhen tempered at 400°F
Elongation at Break 2.0 %2.0 %when tempered at 400°F
Reduction of Area 4.0 %4.0 %when tempered at 400°F
Modulus of Elasticity 207 GPa30000 ksi
Izod Impact Unnotched 298 J220 ft-lbwhen tempered at 400°F
Charpy Impact 5.00 J3.69 ft-lbV Notch, when tempered at 400°F
Charpy Impact, Unnotched 284.7 J
@Treatment Temp. 204 °C
210.0 ft-lb
@Treatment Temp. 400 °F
tempered at 350°F
Abrasion 74.874.8loss in mm3, As-Hardened; ASTM G65
 139.1139.1loss in mm3, Tempered at 650°F; ASTM G65
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.3 µm/m-°C
@Temperature 20.0 - 100 °C
6.28 µin/in-°F
@Temperature 68.0 - 212 °F
 13.6 µm/m-°C
@Temperature 20.0 - 400 °C
7.56 µin/in-°F
@Temperature 68.0 - 752 °F
 14.6 µm/m-°C
@Temperature 20.0 - 700 °C
8.11 µin/in-°F
@Temperature 68.0 - 1290 °F
Transformation Temperature 730 °C1350 °FAc1
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.70 %0.70 %
Chromium, Cr 1.0 %1.0 %
Iron, Fe 95.95 %95.95 %As Balance
Manganese, Mn 0.35 %0.35 %
Nickel, Ni 1.75 %1.75 %
Silicon, Si 0.25 %0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type L6 Low Alloy Tool Steel (UNS T61206)
Latrobe LSS™ L6 Tool Steel (ASTM L6)
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02)
Carpenter O6 Graphitic Tool Steel (AISI O6)
AISI Type H13 Hot Work Tool Steel

NCARN16 / 15855

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.