MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PP Polypropylene, Grey  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle. The chemical and electrical properties are very good. The continuous operating temperatures ranges between 5°C and 100°C.

Properties

  • low weight
  • high heat resistance
  • high tensile strength
  • high surface strength
  • high chemical resistance
  • low oxidation resistance
  • low abrasion resistance
  • brittle in the coldness
  • HF-welding not possible
  • natural color is not weather resistant
Applications
  • pumps
  • valves
  • gaskets
  • supporting stands
  • spacer for the plating
  • particles for toys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccISO 1183
Moisture Absorption at Equilibrium 0.010 %ISO 62
Water Absorption at Saturation 0.20 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 77ISO 868
Tensile Strength at Break 28.0 MPaISO 527
Tensile Strength, Yield 32.0 MPaISO 527
Elongation at Break >= 30 %ISO 527
Elongation at Yield 16 %ISO 527
Modulus of Elasticity 1.635 GPaISO 527
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 50.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
Dielectric Constant 2.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmIEC 60243-1
Dielectric Loss Index 0.00020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°CISO 11359
Melting Point 160 °CDIN EN ISO 3146
Maximum Service Temperature, Air 100 °CUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75
Vicat Softening Point 91.0 °CVST/B/50; ISO 306
Minimum Service Temperature, Air 5.00 °CUL 746B
Glass Transition Temp, Tg 10.0 °CDIN EN ISO 3146
Flammability, UL94 HBUL 94
Oxygen Index 18 %ASTM D2863
 
Compliance PropertiesOriginal ValueComments
FDA YesPhysiological indifference
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistanceno
Bondabilityyes
CKW Resistancelimited
Colorgrey
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceyes
Physiological indifferenceyes, EEC
Resistance Against Hot Wateryes
UV Stabilizationlimited

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics PP Polypropylene, Natural
Reliance Industries METABOLIX PHB
Avient Maxxam® FR PP 301 S HI Polypropylene Copolymer
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Polyram RamOfin PPH308G50 Polypropylene, 50% Glass Fiber, Impact Modified

PGEHR005 / 79842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.