MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Mobilgear 600 Series 629
Categories: Fluid; Lubricant

Material Notes: The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives with circulation or splash lubrication systems. They are formulated from highly refined base stocks and a special additive system that provides an extremely high level of resistance to oxidation and chemical degradation. They have friction-modifying characteristics that reduce power consumption and lower bulk oil temperatures. The Mobilgear 600 Series oils protect against corrosion and rusting, including seawater. They have excellent water separating properties and they are strongly resistant to foaming in service. Mobilgear 600 Series oils are recommended for industrial spur, helical and bevel enclosed gears with circulation or splash lubrication, operating at bulk oil temperatures up to 100ºC. For steel-on-steel applications, Mobilgear 600 Series products are recommended, whereas for bronze-on-steel worm gear applications, Mobil Glygoyle Series or Mobil SHC 600 Series products are recommended. They are particularly suitable for gear sets working under heavy or shock loads. Minimum bulk oil temperatures are governed by the pour point of the oil. Suitable heating may be necessary for the heavier grades at ambient temperatures. Mobilgear 600 oils also find broad application in marine gearing applications. Non gear applications include plain and rolling contact bearings - especially highly loaded and slow speed. Mobilgear 600 Series gear oils are used in a very wide variety of applications in virtually all industrial sectors as well as in marine units. They are the product of choice for many users, worldwide, based on their outstanding performance, equipment protection and application versatility.

Mobilgear 600 lubricants are used in a wide range of industrial and marine applications, especially spur, helical, bevel and worm gearing. Specific applications include: Industrial gearing for conveyers, agitators, dryers, extruders, fans, mixers, presses, pulpers, pumps (including oil well pumps), screens, extruders and other heavy duty applications; Marine gearing including main propulsion, centrifuges, deck machinery such as winches, windlasses, cranes, turning gears, pumps, elevators and rudder carriers; Non-gear applications include shaft couplings, screws and heavily loaded plain and rolling contact bearings operating at slow speeds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/cc
@Temperature 15.6 °C
ASTM D4052
Viscosity Measurement 98Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 150 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.8 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 48ASTM D2783
Four Ball Extreme Pressure, Weld Load 250 kgASTM D2783
Timken Test 65.0 lb
 
Thermal PropertiesOriginal ValueComments
Pour Point -27.0 °CASTM D97
Flash Point 245 °CASTM D92
 
Descriptive Properties
Copper Strip Corrosion1B3 hrs @ 100°C
Demulsibility Time (min)30to 3 mL emulsion @ 54°C
Foam Sequence I, ASTM D10300/0
Foam Sequence II, ASTM D8930/0
FZG Scuffing, DIN 5182, A/8.3/90, Fail Stage12+
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON221 / 75646

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.