Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toughness, excellent puncture resistance, good sealing characteristics and tear resistance. Typical Applications: Heavy duty shipping sacks, lamination films, Ice & frozen food bags, agricultural films, stretch wrap films, etc. Information provided by SABIC. |