PLEXIMID® is a polymethyl methacrylimide (PMMI) product. This molding compound is characterized by its very high heat deflection temperature under load and rigidity. PLEXIMID® molding compounds are particularly suited for injection-molded parts for applications exposed to extreme thermal stress. Information provided by degussa. Evonik Industries is the successor company to Degussa. |