Rigid 4 pound polyurethane foam Key Properties: - Excellent physical properties after RT cure
- Free of mercury, MOCA or TDI
Applications: - For hand-batch and meter-mix processing
- Helmet inserts, structural castings and taxidermy blanks
Cure: 7 days at 77°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |