MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Microtherm Group Hydrophoblic Quilted Panel Filament Reinforced Silica Thermal Insulation Panel, Flexible and Waterproof
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: Microtherm® Hydrophobic Quilted Panel is a truly flexible high temperature microporous insulation panel. It has the additional advantage of being water repellent at low to moderate temperatures. With an outer covering of woven glass cloth the panels offer clean high performance insulation protection for complex shapes.
    Properties
  • Opacified blend of filament reinforced silica
  • Fully flexible high temperature microporous insulation specially treated to repel water during installation.
  • Continuous operation at temperatures up to 1000 °C (1832 °F)
  • Resistant to vibration and system shock loading in use
  • Non combustible
  • Clean to use
  • Simple to cut and shape
  • Environmentally safe. Contains no respirable fibers.
    Typical Applications
  • Used for any application where water or condensation may be present.

Information provided by Microtherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.170 - 0.300 g/cc0.00614 - 0.0108 lb/in³
Thickness 3000 - 15000 microns118 - 591 mil
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  0.680 J/g-°C
@Temperature 0.000 °C
0.163 BTU/lb-°F
@Temperature 32.0 °F
 0.920 J/g-°C
@Temperature 200 °C
0.220 BTU/lb-°F
@Temperature 392 °F
 1.00 J/g-°C
@Temperature 400 °C
0.239 BTU/lb-°F
@Temperature 752 °F
Thermal Conductivity  0.0258 W/m-K
@Temperature 100 °C
0.179 BTU-in/hr-ft²-°F
@Temperature 212 °F
@ 240 kg/m³, cell pitch of 25mm
 0.0283 W/m-K
@Temperature 200 °C
0.196 BTU-in/hr-ft²-°F
@Temperature 392 °F
@ 240 kg/m³, cell pitch of 25mm
 0.0313 W/m-K
@Temperature 300 °C
0.217 BTU-in/hr-ft²-°F
@Temperature 572 °F
@ 240 kg/m³, cell pitch of 25mm
 0.0347 W/m-K
@Temperature 400 °C
0.241 BTU-in/hr-ft²-°F
@Temperature 752 °F
@ 240 kg/m³, cell pitch of 25mm
Maximum Service Temperature, Air 1000 °C1830 °Ffor long term exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Overview of materials for Methacrylate Adhesive
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
Nihon Superior LF-C2 Lead-Free Solder Alloy
Mid-Mountain Materials SILTEX® 18 Amorphous Silica Textile

CMICRO09 / 90051

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.