MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lucite International SW Sanitary Ware Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9898ISO 2039-2
Tensile Strength 70.0 MPa10200 psiISO R527, 5 mm/min
Tensile Modulus 3.20 GPa464 ksiISO R527, 5 mm/min
Flexural Strength 120 MPa17400 psiISO 178, 2 mm/min
Charpy Impact Unnotched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1D
 
Thermal PropertiesMetricEnglishComments
CTE, linear 77.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
42.8 µin/in-°F
@Temperature 32.0 - 122 °F
DIN 5372
Specific Heat Capacity 1.46 J/g-°C0.349 BTU/lb-°F
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FISO 75 Method A
Vicat Softening Point 105 °C221 °FBS2782: 120 C
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 170 °C302 - 338 °Foptimum shaping temperature
 
Descriptive Properties
Color FastnessHot Water - Grey Scale; EN 263
 UV - Grey Scale; ISO 4892-2
Water Absorption (mg)2950 mm2 sample, ISO 62/1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Acrylite® SG Acrylic Sheet, Sign Grade
Plaskolite Optix® SG Sign Grade Acrylic Sheet
SEKISUI SPI KYDEX® 5555 Acrylic/PVC
Spartech Acrylloy F Acrylic Sheet
Overview of materials for PVC, Molded

PLUCIT9402 / 150116

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.