MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Petrothene® NA420000 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Well-balance films with excellent optics, good stiffness and strong heat sealing characters can be produced from this resin.

Regulatory Status
NA 420 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "…in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
NA 420 has excellent drawdown characteristics that yield outstanding output rates. Recommended extrusion conditions are 330°-380°F (166°-194°C) melt temperatures and a blow-up ratio between 1.7-3.0:1. Specific recommendations for the processing of NA 420 can be made only when the end use application, required properties and the processing equipment are known.

Physical Properties
These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D1505
Vinyl Acetate Content 2.5 %2.5 %
Thickness 31.8 microns1.25 mil2:1 BUR; 25 mil die gap
Melt Flow 2.5 g/10 min2.5 g/10 minASTM D1238
Antiblock Level 0.000 ppm0.000 ppm
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 350 %350 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Elmendorf Tear Strength MD 220 g220 gASTM D1922
Elmendorf Tear Strength TD 250 g250 gASTM D1922
Dart Drop Test 80.0 g0.176 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 22.8 MPa3300 psiASTM D882
Film Tensile Strength at Break, TD 16.5 MPa2400 psiASTM D882
1% Secant Modulus, MD 138 MPa20000 psiASTM D882
1% Secant Modulus, TD 172 MPa25000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 4.5 %4.5 %For NA 420-127 (medium-slip, medium antiblock); ASTM D1003
Gloss 73 %73 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 °C375 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQU0487 / 36940

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.