MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Omni Plastics OmniLon™ PA6 GR33 HS BSD10 Nylon 6, 33% Glass reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Optimized ESD control, 33% glass reinforced, heat stabilized; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
Filler Content 33 %33 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 183 MPa26500 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 276 MPa40000 psiASTM D790
Flexural Modulus 11.032 GPa1600.1 ksiASTM D790
Izod Impact, Notched 0.800 J/cm
@Thickness 3.17 mm
1.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+8 - 1.00e+10 ohm1.00e+8 - 1.00e+10 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
@Thickness 3.17 mm
421 °F
@Thickness 0.125 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
@Thickness 3.17 mm
399 °F
@Thickness 0.125 in
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Omni Internal Testing
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 271 °C480 - 520 °F
Middle Barrel Temperature 249 - 282 °C480 - 540 °F
Front Barrel Temperature 249 - 282 °C480 - 540 °F
Nozzle Temperature 249 - 282 °C480 - 540 °F
Melt Temperature 249 - 282 °C480 - 540 °F
Mold Temperature 26.7 - 71.1 °C80.0 - 160 °F
Drying Temperature 82.2 °C180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Back Pressure 0.345 MPa50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omni Plastics OmniLon™ PA6/6 GR43 Nylon 6/6, 43% Glass reinforced
Omni Plastics OmniLon™ PA6/6 GR33 Nylon 6/6, 33% Glass reinforced
Omni Plastics OmniLon™ PA6 GR43 Nylon 6, 43% Glass reinforced
NYCOA 2256 30% Glass Filled Nylon 6

POMNI5050 / 185196

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.