MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Superwool® Plus Board 75 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Rigid boards manufactured using Superwool ® Plus™ fibers, refractory fillers, organic and inorganic binders. Suitable for all applications up to 900°C.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³
Moisture Absorption 2.00 %2.00 %after 2 hours
Loss On Ignition 5.0 %5.0 %after 2 hours @ 800°C
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.000800 GPa0.116 ksiunfired
Compressive Strength 0.400 MPa58.0 psi@ 10% relative deformation; ASTM C165
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0700 W/m-K
@Temperature 400 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-201
 0.0900 W/m-K
@Temperature 500 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 932 °F
ASTM C-201
 0.0900 W/m-K
@Temperature 300 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 572 °F
ASTM C-201
 0.120 W/m-K
@Temperature 600 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-201
 0.130 W/m-K
@Temperature 800 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C-201
Shrinkage 1.0 %1.0 %isothermal heating at classification temperature; ASTM C165
 
Component Elements PropertiesMetricEnglishComments
Al2O3 15.1 %15.1 %
CaO+MgO 19.4 %19.4 %
K2O+Na2O 2.3 %2.3 %
Other 3.8 %3.8 %Fe2O3 + TiO2
SiO2 59.4 %59.4 %
 
Descriptive Properties
Classification Temperature (°C)900
Colorwhite/tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6439 / 203223

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.