MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sinvicomp SFM4200 Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Sinvicomp SFM4200 is a Polyvinyl Chloride Molding Compound available in pellet form.

Availability: Asia Pacific

Features: DEHP Plasticizer; Non-Toxic

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75
@Time 10.0 sec
75
@Time 0.00278 hour
ASTM D2240
Tensile Strength, Yield 12.0 MPa1740 psiASTM D638
Elongation at Break 270 %270 %ASTM D638
 
Processing PropertiesMetricEnglishComments
Processing Temperature 155 - 170 °C311 - 338 °FMixing
Feed Temperature 140 °C284 °F
Nozzle Temperature 160 - 180 °C320 - 356 °F
Mold Temperature 0.000 - 50.0 °C32.0 - 122 °F
 
Descriptive Properties
Heat Stability>30 minOven (374°F), ASTM D2115-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell Ensolite™ IG2 PVC/NBR/CR
Formosa Plastics Formolon® 690F PVC
Formosa Plastics Formolon® 690 PVC
Formosa Plastics Formolon® 685 PVC
Formosa Plastics Formolon® 680H PVC

PTEKNQ1428 / 237919

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.