MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Konson TMTM-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% tetramethylthiuram mono-sulphide, 20% EPDM/EVA binder and dispersing agents

Use Characteristics: A super accelerator Konson® TMTM-80 causes very rapid and scorch-safe vulcanization of natural and synthetic rubbers. Konson® TMTM-80 receives additional activation from basis accelerators, e.g. aldehyde amine and guanidine. Together with sulphenamide and mercapto accelerators in which Konson® TMTM-80 is used as secondary accelerator are of great technical importance. Low sulphur vulcanization provides vulcanizates with good ageing resistance.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective TMTM is assured.

Dosage levels: NR: primary: 0.15 - 0.3 phr + 2 - 3 sulfur secondary: 0.1 - 2.5 phr + 2.5 phr sulfur and 1 phr mercapto accelerator; SBR:primary: 0.25 - 1.5 phr + 2 - 3.5 phr sulfur secondary: 0.1 - 0.75 phr + 2 - 3.5 phr sulfur and 2 phr mercapto accelerator; IIR: primary: 1 - 2 phr + 1 - 2 phr sulfur; NBR: 0.1 - 3 phr + 0.5 - 2 phr sulfur and 1 - 2 phr mercapto accelerator; CR: 0.5 - 1 phr + 0.5 - 1 phr sulphur and 1 - 3 phr guanidine accelerator.

Applications: Cable insulations, light color and white vulcanizates, transparent pure rubber articles.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³
Ash <= 0.50 %<= 0.50 %
Evaporation Loss <= 0.50 %<= 0.50 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 100 °C212 °F
 
Descriptive Properties
AppearanceLight-yellow granules
Content= 98%TMTM
Sieve residue= 0.5 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS019 / 256064

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.