MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Simpact® 60A Tough, Fast Setting Urethanes
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Simpact™ 60A and 85A urethanes are low odor, fast-setting urethane elastomers which offers very high tear strength, impact resistance and wear resistance. Simpact™ urethanes are phthalate free, mercury free and MOCA free. Simpact™ urethanes pour easily. Working time is 4 minutes, handling time is 2 hours and full cure time is 48 hours at room temperature. Cured rubber has exceptional performance characteristics and dimensional stability. Simpact™ urethanes can be colored with SO-Strong™, UVO™ or Ignite™ colorants. Simpact™ urethanes are suitable for making impact resistant props, prototypes and display pieces.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D-1475
Viscosity 1100 cP1100 cPMixed; ASTM D-2393
Linear Mold Shrinkage <= 0.0070 cm/cm<= 0.0070 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D-2240
Tensile Strength, Ultimate 6.83 MPa990 psiASTM D-638
Elongation at Break 400 %400 %ASTM D-412
100% Modulus 2.15 MPa312 psiASTM D-412
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min2.00 hourHandling Time
Pot Life 4.00 min4.00 minASTM D-2471
 
Descriptive Properties
ColorWhite
Mix Ratio100A:94Bby weight
 1A:1Bby volume
Specific Volume25.7[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN051 / 296752

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.