Non-lead stabilized insulation compound recommended for THW and 90C Class 43 applications. UL recognized component for THW and TW. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |