High viscosity nylon copolymer with enhanced impact and high flexibility. Optimized with good melt strength for high line speeds in thin wall sections. Specifically designed for the convoluted tubing industry, but can also be used for other extrusions and some molded parts. Testing conducted on dry as molded specimen at 73°F Information provided by Nylene® Global Polymer Solutions. |