MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M36/NC2 180°C (350°F) Curing Epoxy Matrix, Multiaxial Fabric Laminate (NC2)
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Uses Hexcel NC2 non-crimp fabric based on Tenax HTS fiber; Quasi-isotropic lay-up based on 1072 gsm quadaxial NC2 fabric (267 gsm/ply); Laminates manufactured via resin film infusion

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 432 MPa
@Temperature 23.0 °C
Open Hole TS
 568 MPa
@Temperature 23.0 °C
Tensile Modulus 52.0 GPa
@Temperature 23.0 °C
Compressive Yield Strength 225 MPaCompression strength after impact, 30J
 270 MPaCompression strength after impact, 20J
 291 MPaCompression strength after impact, 6J
 474 MPa
@Temperature 23.0 °C
Open Hole
 587 MPa
@Temperature 23.0 °C
Shear Strength 39.0 MPa
@Temperature 100 °C
Interlaminar shear
 45.0 MPa
@Temperature 23.0 °C
Interlaminar shear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix
Rogers Arlon 51146R020 Silicone Rubber/Fiberglass Laminate
Parabeam Industrie Paraglass 3 3D Glass Fabric
Norplex-Micarta RT571 Epoxy Fiber Glass Laminate Tube, NEMA G-10

PHEXC177 / 98648

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.