MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nouryon Adsee AB 615 Alkoxylated fatty amine
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Adsee AB 615 is an alkoxylated fatty amine

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³
pH 6.0 - 9.06.0 - 9.01% in water
Viscosity 235 cP
@Temperature 20.0 °C
235 cP
@Temperature 68.0 °F
Surface Tension 33 dynes/cm33 dynes/cmaccording to Du Noüy, 0.1%; DIN 53914
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -20.0 °C<= -4.00 °F
Flash Point >= 100 °C>= 212 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 6.0<= 6.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %
 
Descriptive Properties
AppearanceClear to turbid liquid
Equivalent mass1250-1310
Foam Height according to Ross-Miles10 mmafter 5 min, 25°C, 0.05% in de-ionized water
 10 mmafter 5 min, 25°C, 0.05% in Standard Water D
 55 mmimmediately, 25°C, 0.05% in de-ionized water
 57.5 mmimmediately, 25°C, 0.05% in Standard Water D
Wetting power23.5 secaccording to Draves, 25°C, 0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY041 / 285564

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.