MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: PA 6, 60% glass fibers, injection molding, improved flowability

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage, Flow 0.00020 cm/cmPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0020 cm/cm60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.00060 cm/cmPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0020 cm/cm60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 158 MPacond.; ISO 527-1, -2; 5 mm/min
 230 MPad.a.m.; ISO 527-1, -2; 5 mm/min
Elongation at Break 2.5 %d.a.m.; ISO 527-1, -2; 5 mm/min
 3.5 %cond.; ISO 527-1, -2; 5 mm/min
Tensile Modulus 12500 MPacond.; ISO 527-1, -2; 1 mm/min
 20000 MPad.a.m.; ISO 527-1, -2; 1 mm/min
Flexural Strength 390 MPa
@Strain 3 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Modulus 20200 MPad.a.m., 2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 18.0 kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 180-1A
 18.0 kJ/m²
@Temperature -30.0 °C
cond.; ISO 180-1A
Izod Impact, Unnotched (ISO) 90.0 kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 180-1U
 90.0 kJ/m²
@Temperature 23.0 °C
cond.; ISO 180-1U
 90.0 kJ/m²
@Temperature -30.0 °C
d.a.m.; ISO 180-1U
 90.0 kJ/m²
@Temperature -30.0 °C
cond.; ISO 180-1U
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 179-1eU
 95.0 kJ/m²
@Temperature -30.0 °C
d.a.m.; ISO 179-1eU
Charpy Impact, Notched 17.0 kJ/m²
@Temperature 23.0 °C
d.a.m.; ISO 179-1eA
 17.0 kJ/m²
@Temperature -30.0 °C
d.a.m.; ISO 179-1eA
Puncture Energy 3.70 J
@Load <=133 kg,
Temperature -30.0 °C
ISO 6603-2
 4.30 J
@Load <=140 kg,
Temperature 23.0 °C
ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1, -2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1, -2
Melting Point 221 °C10°C/min; ISO 11357-1, -3
Deflection Temperature at 0.46 MPa (66 psi) 222 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 213 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °C
 280 °Cfor test specimens; ISO 294
Mold Temperature 80.0 °Cfor test specimens; ISO 294
 80.0 - 120 °C
Drying Temperature 80.0 °C
Dry Time 2 - 6 hour
Moisture Content 0.060 - 0.20 %residual; Karl Fischer Test
 
Descriptive Properties
ISO Short NameISO 1874-PA 6, GHR, 10-190, GF60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram PlusTek PA108 Nylon6/6.6 Alloy for Injection Molding
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
AdvanSix Capran® Oxyshield® M-OPA (0.60 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Celanese Celstran® PA6-GF60-03 PA6, 60% Glass Reinforced
AdvanSix Capran® Oxyshield® M-OPA (1.0 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film

PLANX0648 / 133611

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.