MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Marco Polo MARPOL LL4M 885 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: MARPOL® LL4M 885 exhibits an excellent flow for high speed injection molding applications such as caps, lids, closures, containers and other items while providing good tear resistance and ESCR.

Recommended Applications: Injection molding - caps, closures, containers, housewares, lids, outdoor and power tools.

Additives: Slip – no, Antiblock - no.

Complies with U.S. FDA 21 CFR 177.1520c 3.1a and European Commission Regulation (EU) No. 10/2011.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.928 g/cc0.0335 lb/in³ASTM D1505
Melt Flow 85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
85 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353ASTM D2240
Tensile Strength at Break 13.0 MPa1890 psiASTM D638
Tensile Strength, Yield 16.0 MPa2320 psiASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus, 1% Secant 535 MPa77600 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 85.0 °C185 °FASTM D1525
Brittleness Temperature -60.0 °C-76.0 °FF50; ASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO154 / 283751

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.