MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Delrin® FG400MTD BLA079 POM-MED(Fe)  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cmISO 294-4, 2577
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 61.0 MPaISO 527-1/-2
Elongation at Break 15 %Nominal; ISO 527-1/-2
Elongation at Yield 8.0 %ISO 527-1/-2
Tensile Modulus 2800 MPaISO 527-1/-2
Flexural Modulus 2700 MPaISO 178
Poissons Ratio 0.37ISO 527-1/-2
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°CISO 11359-1/-2
Melting Point 168 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 205 °CInjection Optimum
 200 - 210 °CInjection
Mold Temperature 90.0 °CInjection Optimum
 80.0 - 100 °CInjection
Drying Temperature 80.0 °C
Dry Time 2.00 - 4.00 hourDehumidified Dryer
Moisture Content 0.20 %
Hold Pressure 80.0 - 100 MPa
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying Recommendedyes
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)8
Part Marking CodePOM-MED(Fe)ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPOM-MED(Fe)ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 100 BK602 POM
KEP Kepital® F10 Standard Grade/High Viscosity Acetal Homopolymer
Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM)
VICTREX™ PEEK 450FE20 Polyetheretherketone, 20% PTFE
Network Polymers Kepital® F10-02

PDSX5148 / 197788

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.