MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DowAksa CarbonBond™ 200-UW Adhesive Putty System
Categories: Polymer; Thermoset; Epoxy

Material Notes: DowAksa CarbonBond™ 200-UW Adhesive Putty System is a high-strength epoxy tack coat that is insoluble in water and non-hygroscopic. It cures rapidly and adheres well to ceramics, concrete, glass, metal, plastic and wood substrates. The product is recommended to prime those substrates and tack pre-saturated carbon fiber reinforcement in place. Its immediate high-tack consistency is advantageous for vertical and overhead applications. CarbonBond™ 200A-UW Putty Resin Part A is color-coded black and CarbonBond™ 200B-UW Putty Hardener Part B is color-coded white. CarbonBond™ 200-UW Adhesive Putty System is recommended as a patching for the leak repair of PCE (Pressure Equipment Container).

Information provided by DowAksa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0377 lb/in³Part B
 1.19 g/cc0.0429 lb/in³Part A
 
Processing PropertiesMetricEnglishComments
Gel Time 20.0 min20.0 min100g
 
Descriptive Properties
ColorBlackPart A
 Dark GreyMixed
 WhitePart B
Mix Ratio100:22 A:BWeight
 4:1 A:BVolume
ViscosityPastePart A
 PastePart B
 Thixotropic PasteMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWAK986 / 287933

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.