MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monomer, is polymerized by low pressure or high pressure method and then can be maintained as high density (PE-YY 0,941 and 0,965 g/cm³) or low (normal) density polyethylene(PE-NY 0,914 and 0,925 g/cm³). Other differences of various PE types are according to their melting degrees and opposite proportional connection occurs according to their relative molecular weights. In other words, when its melting degree is at the lowest level, its relative molecular weight is at the highest level and e.g. its mechanical specialties are the best.

POLIPOLEN has quite a low density. Its flexibility rate is high and it is resistant to strokes even at low temperatures. It has a very high molecular weight(molecular chain length). It has a high corrosion resistance because of its high molecular chain. According to the results of the "sand slurry" corrosion test which is made as per "DIN" standards, POLIPOLEN 1000 , has shown the highest corrosion resistance among the solid materials( e.g. steels, tree, other engineering plastics.)

PROPERTIES OF POLIPOLEN®:

  • Very high stroke resistance
  • Very high corrosion resistance
  • Very high chemical resistance
  • Getting lubricated itself and slick
  • Excellent electrical resistance
  • Quietness while processing and reducing vibrations
  • Easy processing
  • Low friction rate
  • Very low water absorption
GENERAL USAGE AREAS OF POLIPOLEN®:
  • Coal warehouses and conveyor systems
  • Gutters
  • Chain conveyor guides
  • Elevators
  • Electric power stations
  • Cement industry
  • Lime industry
  • Palister industry
  • Food industry
  • Cutting and chopping plates
  • Chopping blocks
  • Conveyor screws
  • Sliding elements
  • Flat guides
  • Profiles
  • Bobbins
  • Star and screw conveyors
  • Elevator systems
  • Sliding bearings
  • Gears
  • Motor landing plates
  • Stopper valves
  • Closing claps
  • Acid pumps
  • Filters

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity >= 0.950 g/cc>= 0.950 g/ccISO.1183 DN.53479
Water Absorption <= 0.020 %<= 0.020 %ISO.62 DN.53495
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 7060 - 70DN.53505
Ball Indentation Hardness 45.0 MPa6530 psiISO.2039-2
Tensile Strength at Break >= 40.0 MPa>= 5800 psiISO.527 DN.53455
Tensile Strength, Yield 20.0 - 25.0 MPa2900 - 3630 psiISO.527 DN.53455
Elongation at Break >= 500 %>= 500 %ISO.527 DN.53455
Elongation at Yield 12 %12 %ISO.527 DN.53455
Modulus of Elasticity >= 0.800 GPa>= 116 ksiISO.178 DN.53452
Charpy Impact, Notched 5.00 J/cm²23.8 ft-lb/in²ISO.179 DN.53453
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 5.00e+16 ohm-cm>= 5.00e+16 ohm-cmISO.167 DN.53482
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmISO.167 DN.53482
Dielectric Strength >= 50.0 kV/mm>= 1270 kV/inISO.243 DN.53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
DN.53752
Melting Point 130 - 133 °C266 - 271 °F
Maximum Service Temperature, Air 70.0 °C158 °FISO.75 DN.53461
 
Descriptive Properties
Corrosion< 400 %DN.58836 Sand Slurry Test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum, Al
Formosa Plastics Formolene® LH5204 Injection Molding HDPE
Formosa Plastics Formolene® LH5206 Injection Molding HDPE
Formosa Plastics Formolene® LH5212 Injection Molding HDPE
Formosa Plastics Formolene® LH5240 Injection Molding HDPE

PPOLIM08 / 56974

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.