MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Tacna® EP Polyurea Grease NLGI Grade 2
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off-road equipment, fleet and commercial applications. It has excellent mobility at low temperatures. Applications Include:
  • Fleet/Off-Road Equipment:
    • Universal joints
    • Heavy-duty truck wheel bearings
    • Water pumps
    • Idler pulleys
  • Industrial Applications:
    • Roller bearing requiring EP grease (temperatures up to 350°F (177°C))

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 1251 SUSBase Oil Property
Saybolt Viscosity at 210°F 94 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 235 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 18 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 70
Four Ball Extreme Pressure, Weld Load 500 kg
Four Ball Wear 0.380 mmWear Scar
Penetration P(60), 1/10 mm 286
Timken Test 55.0 lb
 
Thermal PropertiesOriginal ValueComments
Dropping Point 542 °F
 
Descriptive Properties
ColorGreen
Rust TestPass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON231 / 75268

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.