MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
LyondellBasell Koattro KT AR 05 Plastomer  (discontinued **)
Categories: Polymer; Film; Thermoplastic

Material Notes: Koattro is a novel family of high-molecular-weight plastomers. Koattro KT AR05 is a novel plastomeric material based on LyondellBasell technology. The product shows an excellent compression set performance which is highly compatible with Polypropylene. Blended with PP it enhances softness, elastic recovery, elongation at break and impact resistance whilst improving transparency and reducing stress whitening. Blended at low concentrations in PP, Koattro KT AR05 enhances also the thermal bonding strength. Koattro KT AR05 is available in free flowing pellet form. Applications: Appliances, Automotive Parts, Coatings, Protective, Color Concentrates, Industrial, Polymer Modifier, Products for Use in Property Modification, Sealants, Surface Protection Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccISO 1183-1
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87ISO 868
Tensile Strength at Break 12.0 MPaspecimens conditioned for 10 days at 23°C; ISO 8986-2
Elongation at Break >= 400 %specimens conditioned for 10 days at 23°C; ISO 8986-2
Tensile Modulus 19.0 MPaspecimens conditioned for 10 days at 23°C; ISO 527-1,-2
Flexural Modulus 25.0 MPaspecimens conditioned for 10 days at 23°C; ISO 178
Charpy Impact, Notched 5.10 kJ/m²
@Temperature -20.0 °C
ISO 179
 NB
@Temperature 23.0 °C
ISO 179
 NB
@Temperature 0.000 °C
ISO 179
Compression Set 42 %
@Temperature 70.0 °C
25% deformation; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 114 °CTm1; ISO 11357-3
 
Descriptive Properties
Processing MethodBlown Film, Calendaring, Cast Film, Compression Molding, Injection Molding.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQT7598 / 219235

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.