MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Label-Lyte® 65 LIM-301 White Opaque OPP Film for Injection Mold Label Applications  (discontinued **)
Categories: Polymer; Adhesive; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: White, treated, polypropylene film designed for injection mold labeling. It provides the right combination of roughness, anti-static, printability, cutting, and stiffness properties for this demanding application. The treated print surface is designed for conventional and UV-cured offset lithography, solvent flexo, and gravure printing. This film has a smooth glossy appearance after molding, resulting in outstanding container graphics.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 66.0 microns2.60 mil
Coating Weight >= 46.1 g/m²>= 28.8 lb/ream520
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 180 %180 %510
Film Elongation at Break, TD 65 %65 %510
Coefficient of Friction 0.250.25untreated side; 430
 0.300.30treated side; 430
Film Tensile Strength at Break, MD 100.77 MPa14615 psi510
Film Tensile Strength at Break, TD 151.15 MPa21923 psi510
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 3.5 %
@Temperature 135 °C
3.5 %
@Temperature 275 °F
438
Shrinkage, TD 1.3 %
@Temperature 135 °C
1.3 %
@Temperature 275 °F
438
 
Optical PropertiesMetricEnglishComments
Gloss 10 %10 %untreated surface; 442
 50 %50 %treated surface; 442
Transmission, Visible 15 %15 %417
 
Descriptive Properties
Gurley Stiffness, MD, mgf23
Gurley Stiffness, TD, mgf39
Yield, in2/lb15000

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 4072 Polypropylene, Injection Grade
Aclo Accutech Polypropylene Copolymer CP0436C40L1 Calcium Reinforced
Bamberger Polymers Bapolene® 4082 Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 5083C Polypropylene, Injection Grade
Braskem PH 0952 HOMO Polypropylene Homopolymer

PEXB486 / 37791

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.