MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BorsodChem ONGROVIL S-5064 Suspension PVC-Resin
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Uncompounded

Material Notes: S-5064 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It retains its excellent pourability even after compounding.

Field of application: Ongrovil S-5064 is primarily suitable for rigid applications. It is recommended for extruded or calendered films and sheets as well as for injection molding or production of hollow articles.

Information provided by BorsodChem Rt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.530 - 0.590 g/ccISO 60:1977
Particle Size 63 µm5% below
 250 µm1% above
Collected Volatile Condensable Material <= 0.30 %ISO 1269:1980
 
Descriptive Properties
# of Impuritiesmax. 20 pcs/9dm2
K-Value64±1
Pouring Time, sec (max)23.5
Residual Vinyl-Chloride ContentMax 1 mg/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary PVC AG K580A Q2 Polyvinyl Chloride Thermoplastic
Geon® Performance Solutions Vinyl Flexible C80A0
Geon® Performance Solutions Vinyl Flexible R 980A Polyvinyl Chloride, Flexible
BorsodChem ONGROVIL S-5070 Suspension PVC-Resin
BorsodChem ONGROVIL S-494 Suspension PVC-Resin

PBORS03 / 27527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.