MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Omni Plastics OmniPro™ CPP XE72A BK17 Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: High impact, electrostatic dissipative; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D792
Melt Flow 4.0 g/10 min4.0 g/10 minASTM D1248
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Flexural Strength 26.0 MPa3770 psiASTM D790
Flexural Modulus 1.207 GPa175.1 ksiASTM D790
Izod Impact, Notched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
@Thickness 3.17 mm
219 °F
@Thickness 0.125 in
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Omni Internal Testing
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 204 - 249 °C400 - 480 °F
Middle Barrel Temperature 216 - 260 °C420 - 500 °F
Front Barrel Temperature 216 - 260 °C420 - 500 °F
Nozzle Temperature 216 - 260 °C420 - 500 °F
Melt Temperature 216 - 260 °C420 - 500 °F
Mold Temperature 26.7 - 60.0 °C80.0 - 140 °F
Drying Temperature 82.2 °C180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.20 %<= 0.20 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POMNI5066 / 185212

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.