Description: Apcotex GC 950A is a specialty silicon free carboxylated styrene butadiene latex, with higher operating viscosity, specifically to make polymer coated gloves of natural rubber latex with excellent donning properties. It is manufactured by employing state-of-the-art emulsion polymerization technology ensuring product consistency. Advantages: - Excellent adhesion to nitrile rubber gloves
- Recommended to make powder free nitrile rubber gloves
- Recommended to make silicon free polymer coated nitrile rubber gloves
- Provides uniform film coating on glove surface
- Provide excellent smoothness at donning side
- Easily miscible with water at any proportion
- Offers higher operating viscosity for coating process
Information provided by Apcotex Industries Limited |