MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese SO.F.TER Technoprene® 3K8 Glass-Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Copolymer Technoprene® 40% Glass-Reinforced Polypropylene

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
Water Absorption 0.020 %
@Temperature 23.0 °C,
Time 86400 sec
0.020 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inSO.F.TER Method
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 MPa11600 psiASTM D638
Flexural Strength 125 MPa18100 psiASTM D790
Flexural Modulus 7.30 GPa1060 ksiASTM D790
Izod Impact, Notched  1.55 J/cm
@Temperature -20.0 °C
2.90 ft-lb/in
@Temperature -4.00 °F
ASTM D256/A
 2.00 J/cm
@Temperature 23.0 °C
3.75 ft-lb/in
@Temperature 73.4 °F
ASTM D256/A
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+15 ohm1.00e+15 ohmASTM D257
Dielectric Constant 2.52.5ASTM D150
Comparative Tracking Index >= 650 V>= 650 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 - 60.0 µm/m-°C22.2 - 33.3 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 147 °C297 °FASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOFS829 / 162293

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.