MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Yuyao Zhonga ABS FRML ABS flame retardant masterbatch
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Flame-retardant masterbatch of ABS: keeping its good mechanical properties, ageing resistance, thermal stability, good processability and so on after adding the masterbatch, and the flame retardant grade could be changed from UL-94,V0,V1,V2 to HB. The mixture of flame-retardant masterbatch and ABS can replace flame-retardant ABS to decrease production cost, what can be used for TV shells, household appliances shells, low voltage electric switch, electric plug-in unit, communications equipments, luminaire, mining electric apparatus parts, etc.

Information provided by Yuyao Zhongfa Engineering Plastics CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.60 mm
Proportion: 10%
 V-2
@Thickness 1.60 mm
Proportion: 15%
 V-1
@Thickness 1.60 mm
Proportion: 20%
 V-0
@Thickness 1.60 mm
Proportion: 25%
 
Processing PropertiesOriginal ValueComments
Processing Temperature 185 - 215 °CInjection Temp
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 85.0 - 90.0 °C
Dry Time 2.00 - 3.00 hour
Injection Pressure 60.0 - 90.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PYUYZ073 / 281866

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.