MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.

Application examples: Thin shrink film for food packaging (coextrusion, lamination...), stretch film.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.929 g/cc0.929 g/ccISO 1183
Vinyl Acetate Content 9.0 %9.0 %
Thickness 40.0 microns1.57 milfor samples tested on this data sheet
 20.0 - 100 microns0.787 - 3.94 milpossible range, depending on extrusion conditions
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 7.80 MPa1130 psiISO 527-3
Film Tensile Strength at Yield, TD 6.50 MPa943 psiISO 527-3
Film Elongation at Break, MD 380 %380 %ISO 527-3
Film Elongation at Break, TD 570 %570 %ISO 527-3
Modulus of Elasticity 0.100 GPa14.5 ksiISO 527-2
Elmendorf Tear Strength, MD 3.10 g/micron78.7 g/milISO 6383-2
Elmendorf Tear Strength, TD 3.60 g/micron91.4 g/milISO 6383-2
Dart Drop Test 400 g0.882 lbISO 7765-1
Film Tensile Strength at Break, MD 29.0 MPa4210 psiISO 527-3
Film Tensile Strength at Break, TD 24.0 MPa3480 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 97.0 °C207 °FISO 11357
Vicat Softening Point 79.0 °C174 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze 3.5 %3.5 %ISO 14782
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 180 °C302 - 356 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade
ExxonMobil Escorene® LD 713.93 Cast Film Resin
ExxonMobil EXACT™ 4150 Plastomer
Total 4320 Polypropylene, Impact Copolymer

PTOTAL703 / 130428

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.