MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic

Material Notes: AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable to simple shapes and thermo-formable to complex three-dimensional curves, and is nonfriable. AIREX® R63 is a core material for dynamically loaded and shock absorbing sandwich structures.

Characteristics

  • Good impact strength (non-brittle failure mode)
  • Easy to thermoform (cold and hot)
  • Dimensionally stable
  • Excellent fatigue resistance
  • Outstanding core-to-skin adhesion
  • Non biodegradable
  • Good sound and thermal insulation
Applications
  • Marine: Hull bottoms, hull sides
  • Road and Rail: Front-ends, side skirts, crash belts
  • Aircraft: Explosion proof cargo containers
  • Recreation: Surf boards, canoes, kayaks
  • Industrial: Containers, shelters, helmets
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.140 g/ccaverage; ISO 845
 0.125 - 0.170 g/cctypical range; ISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 2.20 MPain the plane; ISO 527 1-2
 2.40 MPaaverage; in the plane; ISO 527 1-2
Elongation at Break >= 75 %shear; ISO 1922
 80 %average; shear; ISO 1922
Tensile Modulus >= 80.0 MPain the plane; ISO 527 1-2
 90.0 MPaaverage; in the plane; ISO 527 1-2
Compressive Strength >= 1.30 MPaperpendicular to plane; ISO 844
 1.60 MPaaverage; perpendicular to plane; ISO 844
Compressive Modulus >= 100 MPaperpendicular to plane; DIN 53421
 110 MPaaverage; perpendicular to plane; DIN 53421
Shear Modulus >= 0.0350 GPaASTM C393
 0.0370 GPaaverage; ASTM C393
Shear Strength >= 1.60 MPaISO 1922
 1.85 MPaaverage; ISO 1922
Charpy Impact, Notched 6.50 kJ/m²DIN 53453
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0390 W/m-KISO 8301
 
Descriptive Properties
Colorbrownish yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam
3A Composites Core Materials AIREX® PXc.420 Fiber-Reinforced Structural Foam
3A Composites Core Materials AIREX® PXc.245 Fiber-Reinforced Structural Foam
3A Composites Core Materials AIREX® PXw.420 Fiber-Reinforced Structural Foam Panel
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam

PZ3AC024 / 108513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.