MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Suqian Unitechem Antioxidant B225
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS NO.: 6683-19-8 31570-04-4

Properties: Antioxidant B225 is a kind of compound components, including antioxidant 1010 and 168. Soluble in benzene, hexane, ethyl acetate, insoluble in water.

Uses: Good synergistic of antioxidant 1010 and 168, can retard heated degradation and oxidative degradation of polymeric substances during processing and in end applications. It can be widely used for PE, PP, PC, ABS resin and other petro-products. The amount to be used may be 0.1-0.8%.

Information Provided by Suqian Unitechem Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.50 %
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 96 %425nm
 >= 97 %500nm
 
Descriptive Properties
AppearanceWhite powder
Content of Antioxidant 1010 (%)45.0-55.0
Content of Antioxidant 168 (%)45.0-55.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUQI16 / 103999

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.