MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® PP 2500/4 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound 2500/4 is a mineral filled modified polypropylene. Typical material properties include high flow, very high impact, good stiffness, low shrinkage and CLTE. Typical applications of this grade are in automotive exterior such as automotive bumpers. It can be used in painted and unpainted applications with UV stabilization added on demand. SABIC® PPcompound 2500/4 is a designated automotive grade. IMDS ID: 16485974

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³Injection molded sample ISO527-1A; ISO 1183
Filler Content 10 %10 %SABIC method
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/inInjection molded plaque 65x65x3.2mm; SABIC method
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
13 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ISO 868
Tensile Strength at Break 21.0 MPa3050 psiISO 527/1A
Tensile Strength, Yield 20.0 MPa2900 psiISO 527/1A
Elongation at Break >= 500 %>= 500 %ISO 527/1A
Tensile Modulus 1.05 GPa152 ksiISO 527/1A
Flexural Modulus 1.10 GPa160 ksiISO 178/1A
Izod Impact, Notched (ISO) NBNBISO 180/1A
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 180/1A
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched NBNBISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear  60.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
33.3 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
 70.0 µm/m-°C
@Temperature -30.0 - 100 °C
38.9 µin/in-°F
@Temperature -22.0 - 212 °F
ISO 11359-2
 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 176 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FISO 75
Vicat Softening Point 125 °C257 °Fat 10 N (VST/A); ISO 306/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11408 / 244875

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.