MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Dylark® FG2500 High-Heat Styrenic Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; SMA Polymer; Styrene-Maleic Anhydride (SMA), Heat Resistant

Material Notes: Product Description and Features: Styrenic copolymer with high-heat resistance, high-impact strength and good toughness. Resins used in food grade sheet extrusion and injection molding applications. Microwavable Resin

Processing: Contact NOVA Chemicals technical personnel for processing assistance. Data presented here is based on test results from a limited number of samples and may change as additional manufacturing data is obtained.

Availability: Available in boxes, truckloads, and railcars.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 in/inASTM D 955
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 26.0 MPa0.2 inches/minute; ASTM D 638
Tensile Strength, Yield 28.0 MPa0.2 inches/minute; ASTM D 638
Elongation at Break 20 %0.2 inches/minute; ASTM D 638
Tensile Modulus 2070 MPa0.2 inches/minute; ASTM D 638
Flexural Strength 57.0 MPaat <5% Strain, flexural testing speed of 0.5 inches/minute; ASTM D 790
Flexural Modulus 2140 MPaFlexural testing speed of 0.5 inches/minute; ASTM D 790
Izod Impact, Notched 5.00 ft-lb/in
@Thickness 3.17 mm
ASTM D 256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
@Thickness 3.17 mm
Annealed; ASTM D 648
Vicat Softening Point 253 °F
@Load 1.00 kg
Rate B; 120°C/hr; ASTM D 1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic
NOVA Chemicals Dylark® 480P12 High Performance Glass Filled Styrenic
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin

PNOV856 / 108464

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.