Description: This product is an industrial amine functionalized polydimethylsiloxane polymer. Key Features - Detergent Resistant
- Long Lasting Shine
- Improved water repellency
- Abrasion resistance
Key Applications- Automotive care
- Polishing applications
- Mold release
- Top coat applications
Application: ICM SF 729P is a 100% active Aminofunctional Polydimethylsiloxane. It uses the polar nature of Aminofunctional silicones to cause a film to deposit and adhere to surfaces including paint, chrome, aluminum and textiles.Information provided by CHT Group |