MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Manganese Bronze Alloy, UNS C86350, M01 Temper, Castings
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Fabrication Properties: Excellent Suitability – Soldering, Brazing; Good Suitability – Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.19 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 360 - 440 MPa52200 - 63800 psi
 400 MPa58000 psiTypical
Tensile Modulus 105 GPa15300 ksi
Modulus of Rigidity 37.2 GPa5400 ksi
Compressive Strength 2400 MPa348000 psi0.1 in. set/in.
Poissons Ratio 0.420.42
Machinability 65 %65 %
Shear Strength 220 MPa31900 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000200 ohm-cm0.0000200 ohm-cm8.52% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.5 µm/m-°C
@Temperature 20.0 - 100 °C
9.17 µin/in-°F
@Temperature 68.0 - 212 °F
 19.6 µm/m-°C
@Temperature 20.0 - 200 °C
10.9 µin/in-°F
@Temperature 68.0 - 392 °F
 20.2 µm/m-°C
@Temperature 20.0 - 300 °C
11.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.410 J/g-°C0.0980 BTU/lb-°F
Thermal Conductivity 3.11 W/m-K21.6 BTU-in/hr-ft²-°F
Melting Point 871 - 921 °C1600 - 1690 °F
Solidus 871 °C1600 °F
Liquidus 921 °C1690 °F
Annealing Point >= 720.0 °C>= 1328 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 300 °C572 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.30 - 1.1 %0.30 - 1.1 %
Copper, Cu 60 - 64 %60 - 64 %
Iron, Fe <= 1.0 %<= 1.0 %
Lead, Pb <= 0.090 %<= 0.090 %
Magnesium, Mg <= 0.10 %<= 0.10 %
Manganese, Mn 2.0 - 5.0 %2.0 - 5.0 %
Nickel, Ni <= 0.50 %<= 0.50 %
Tin, Sn <= 0.80 %<= 0.80 %
Zinc, Zn 28.4 - 37.7 %28.4 - 37.7 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC86350x1 / 292556

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.