Hostacom TRC 2125N E is a 6% talc filled PP copolymer compound, with superior flowability, low odor and low emissions, high scratch resistance combined with low density & good dimensional stability. Advanced technologies allowed for a significant reduction of mineral filler content which contributed to the reduction of final part weight and improvement of scratch resistance performances. This product is also available in other colors, new colors can be developed depending on customer requirements. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Excellent Processability; Excellent Stiffness; Good Abrasion Resistance; Good Color Stability; Good Impact Resistance; Good Surface Finish; High Flow; Low Density; Low to No Odor; Low VOC Emission; Scratch Resistant; UV Resistant Information provided by LyondellBasell. |