MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo TYRIL™ 905 UV Styrene-Acrylonitrile
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes: TYRIL™ styrene-acrylonitrile (SAN) resins are designed to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications. The key property of TYRIL 905 is its superior water-clear clarity compared to other SAN resins and a high thermal stability that results in consistent color (reduced yellowing). TYRIL 905 is designed for applications demanding chemical and heat resistance and offers good processability. TYRIL 905 represents a technology breakthrough in trace-color reduction. Its thermal stability and exceptionally low base color make it a product especially suited for self-coloring. The UV-stabilized version exhibits excellent weatherability, suitable in particular for lighting applications.

Applications:

  • Large appliances: transparent kitchen parts
  • Lighting applications: louvers and covers
  • Automotive: taillight lenses and reflectors
  • Cosmetic packaging: water-clear, thick-wall applications

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183/B
Apparent Bulk Density 0.690 g/ccISO 60
Melt Flow 5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 13 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 82ASTM D785
Tensile Strength at Break 68.0 MPa5 mm/min; ASTM D638
 68.0 MPaISO 527-2/5
Tensile Modulus 3600 MPaISO 527-2/5
Flexural Strength 95.0 MPaASTM D790
Izod Impact, Unnotched (ISO) 12.0 kJ/m²ISO 180
Charpy Impact Unnotched 15.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 9.10 kV/mmIEC 60243-1
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°CDIN 53752
Specific Heat Capacity 1.38 J/g-°CASTM D2766
Deflection Temperature at 1.8 MPa (264 psi) 100 °CAnnealed; ISO 75-2/A
Vicat Softening Point 101 °CISO 306/B50
 110 °CISO 306/A120
Flammability, UL94 HB
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo TYRIL™ 867 E Styrene-Acrylonitrile

PTRINS9103 / 197575

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.